gelcoat on the sheer stripe is badly oxidized
Viewed: 427 times.
|
oxidized
Viewed: 321 times.
|
original color behind the registration numbers
Viewed: 298 times.
|
needs to be wetsanded
Viewed: 273 times.
|
|
after pressure washing as much of the bottom paint off as possible
Viewed: 300 times.
|
|
|
this is the result after wetsanding with 400 grit. in hindsight I should have started with the mirka abralon 500 and then went to the 1000. I was not able to fully get these swirls out
Viewed: 239 times.
|
this stuff is where I really started to see the difference
Viewed: 284 times.
|
|
|
|
|
|
|
|
you may not see them in this photo, but the swirls from the 400 grit are still there. however, this boat now looks really good, and it was looking pretty sad
Viewed: 262 times.
|
taping off for the epoxy coats after roughsanding the old bottompaint off (sucked)
Viewed: 251 times.
|
after first coat of the epoxy
Viewed: 270 times.
|
rolling on the pettit hydrocoat
Viewed: 273 times.
|
hammerhead emerges from the \'hospital tent\' as I was calling it
Viewed: 368 times.
|